Qiu, J.; Zeng, G.; Ha, M.-A.; Hou, B.; Mecklenburg, M.; Shi, H.; Alexandrova, A. N.; Cronin, S. B. Microscopic Study of Atomic Layer Deposition of TiO₂ on GaAs and Its Photocatalytic Application. Chem. Mater. 2015, 27 (23), 7977–7981. Download

Qiu, J.; Zeng, G.; Ha, M.-A.; Hou, B.; Mecklenburg, M.; Shi, H.; Alexandrova, A. N.; Cronin, S. B. Microscopic Study of Atomic Layer Deposition of TiO₂ on GaAs and Its Photocatalytic Application. Chem. Mater. 2015, 27 (23), 7977–7981. Download

Scroll to Top